Causes and prevention methods of incomplete penetration of argon arc welding gun

Views: 15     Author: Site Editor     Publish Time: 2022-11-14      Origin: Site

facebook sharing button
twitter sharing button
line sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
sharethis sharing button

The main reasons for incomplete penetration are small groove angles, too small gaps or too thick blunt edges, too small flame energy rate or too fast welding speed, too fast heat dissipation rate of the weldment, and the existence of the molten pool for a short time. Can not be fully fused with the base metal. The prevention method is to choose the correct groove form and proper welding assembly gap, and eliminate the dirt and slag on both sides of the groove and between the welding layers. Choose the appropriate flame energy rate and welding speed, which is good for fast heat conduction and large heat dissipation surface. Weldments require preheating before welding or heating during welding.

Related News

About Us

HALANSM is a leader in the design and manufacture of robotic and manual MIG/plasma torches and consumables in China.

We look forward to working with you to create value for customers around the world.

Follow Us
The premier manufacturer in the welding and cutting industry in China
Copyright © 2022​​​​​​​ Changzhou Haran Machinery Technology Co., Ltd.